Copper | 99.2% | ||
Phosphorus | 0.004-0.012% | ||
Tellurium | 0.4-0.7% | ||
Tensile Strength | RmMpa | ≥330 | |
Yield Strength | δ0.5Mpa | 205 | |
Elongation | % | ≥10 | |
Coefficient of elasticity | Mpa | 117000 | |
Electrical Conductivity | %IACS | ≥90 | |
Hardness | HRB | 35-55 |
Shape | Condition | Size |
Straight Round Rod/ Wires | hard/half hard | Φ2-15mm |
Straight Round Rod | hard/half hard | Φ3-90mm |
Flat Bars/ Plates/ Sheets | hard/half hard | a2-8*b2-150mm |