The pressure welding is to press the copper foil laminations together, using molecular diffusion welding, and forming by high-current heating and pressure welding.
Copper foil: 0.03mm to 0.3mm thick.
The contact surface can be tinned or silver plated according to users’ requirements.
Copper content: 99.98%
Electrical conductivity: 57
Tensile strength: 379
Technical parameter table of pressure welding / brazing
ED copper | Section mm2
| A mm | B mm | S mm | L mm | H mm | Holes Diameter mm | End drilling | Current capacity A |
PWR 200/180/40 | 200 | 50 | 40 | 5 | 180 | 40 | 13 | W1 | 600 |
PWR 200/230/40 | 200 | 50 | 40 | 5 | 230 | 40 | 13 | W1 | 800 |
PWR 320/230/40 | 320 | 50 | 40 | 8 | 230 | 43 | 13 | W1 | 800 |
PWR 400/230/40 | 400 | 50 | 40 | 10 | 230 | 45 | 13 | W1 | 900 |
PWR 250/250/50 | 250 | 60 | 50 | 5 | 250 | 45 | 13 | W1 | 700 |
PWR 400/250/50 | 400 | 60 | 50 | 8 | 250 | 48 | 13 | W1 | 950 |
PWR 500/250/50 | 500 | 60 | 50 | 10 | 250 | 50 | 13 | W1 | 1100 |
PWR 480/300/60 | 480 | 90 | 60 | 8 | 300 | 70 | 13 | W2 | 1100 |
PWR 600/300/60 | 600 | 90 | 60 | 10 | 300 | 70 | 13 | W2 | 1200 |