ASTM Testing and Evaluation Results for 25mm decking
Test Method | Characters | Result |
ASTM D638 | Tensile test | 18.0 MPa |
ASTM E831 | Coefficient of linear thermal expansion | 40.5 μm/m C |
ASTM D256 | Impact resistance | 33.7 J/m Type of break: Complete Break |
ASTM D6109 | Flexural strength | MOR: 29.3 Mpa MOE: 3715 Mpa |
ASTM D790 | Flexural properties | MOR: 34.1 Mpa MOE: 2503Mpa |
ASTM D4060 | Abrasion resistance | Weight loss: 0.07g |
ASTM D6007 | Formaldehyde test | ND² |