Introduction:
an adhesive mortar for quick and secure laying of aerated lightweight concrete blocks and panels. For thin-bed laying with increased productivity and resistance against water penetration. It is specially formulated to give good workability, adhesion and water retentivity to facilitate optimum strength development.
A high quality cementitious adhesive specifically formulated for installation of AAC products such as blocks, panels and lintels. Backed by extensive testing and historical performance, the use of the adhesive ensures optimum compatibility and performance of the completed installation including strength and fire rating, SA mortar can be applied for interior and exterior use on horizontal and vertical surfaces.
Feature:
1) Weatherproof, and resistant to frost after hardening
2) Strong friction bond due to the adjustment of the water retention properties to suit the absorbency characteristics of the aerated concrete
3) NO rapid loss of water, or loss of water to the subsurface
4) Easy correction of brick position after the brick has been laid
5) Good workability
6) Fulfills the mortar requirements for subsequent thin plastering
Application:
1) Special dry mortar for bonding extremely absorbent aerated-concrete high-precision units and elements
2) For thin mortar joints, 1 to 3 mm thick
3) For application using a mortar sledge or thin-bed roller.
4):Can be used to the decorative face brick in the cold area and plant,used as brick gas.wall brick adhesive uses high quality concrete as raw material, its a kind of high class adhesive material improved by science method, all kinds of property indexes accord with JC890-2001 standard
5):Good waterproof performance, can avoid wall permeating effectively if uses this product sticking bricks
6):Brick and the wall can stick together without wetness, dramatically improve process efficient
Technical Date:
Intensity level |
M2.5 M15 M5.0 M20 M7.5 M25 M10 M30 |
Consistency (mm) |
Less than or equal to 90 |
Water retention ( % ) |
Greater than or equal to 90 |
28 days compressive strength (Mpa) |
≥Its intensity level |
28 days Shrinkage ( % ) |
≤0.5 |