Size Range | ||
Wire | 0.05-8.0mm | |
Rod/Bar | 8.0-200mm | |
Strip | (0.05-0.5)*(5-200)mm | |
Plate | custom made | |
Tube | custom made |
Item | Inconel 600 | Inconel 601 | Inconel 617 | Inconel 625 | Inconel690 | Inconel718 | Inconel X750 | Inconel 825 |
C | ≤0.15 | ≤0.1 | 0.05-0.15 | ≤0.08 | ≤0.05 | ≤0.08 | ≤0.08 | ≤0.05 |
Mn | ≤1 | ≤1.5 | ≤0.5 | ≤0.35 | ≤0.5 | ≤0.35 | ≤1 | ≤1 |
Fe | 6-10 | rest | ≤3 | rest | 7-11 | rest | 5-9 | ≥22 |
P | ≤0.015 | ≤0.02 | ≤0.015 | -- | -- | -- | -- | -- |
S | ≤0.015 | ≤0.015 | ≤0.015 | ≤0.015 | ≤0.015 | ≤0.01 | ≤0.01 | ≤0.03 |
Si | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.35 | ≤0.5 | ≤0.35 | ≤0.5 | ≤0.5 |
Cu | ≤0.5 | ≤1 | -- | ≤0.3 | ≤0.5 | ≤0.3 | ≤0.5 | 1.5-3 |
Ni | ≥7.2 | 58-63 | ≥44.5 | 50-55 | ≥58 | 50-55 | ≥70 | 38-46 |
Co | -- | -- | 10-15 | ≤10 | -- | ≤1 | ≤1 | -- |
Al | -- | 1-1.7 | 0.8-1.5 | ≤0.8 | -- | 0.2-0.8 | 0.4-1 | ≤0.2 |
Ti | -- | -- | ≤0.6 | ≤1.15 | -- | -- | 2.25-2.75 | 0.6-1.2 |
Cr | 14-17 | 21-25 | 20-24 | 17-21 | 27-31 | 17-21 | 14-17 | 19.5-23.5 |
Nb+Ta | -- | -- | -- | 4.75-5.5 | -- | 4.75-5.5 | 0.7-1.2 | -- |
Mo | -- | -- | 8-10 | 2.8-3.3 | -- | 2.8-3.3 | -- | 2.5-3.5 |
B | -- | -- | ≤0.006 | -- | -- | -- | -- | -- |
Density | 8.28 g/cm3 |
Ultimate Strength (≥ MPa) | 910 |
Tensile Strength σb/MPa | 910 |
Elongation δ5 (%) | 30 |
Yield Strength σp0.2/MPa | 550 |
Melting point | 1393-1427℃ |
Specification | ||||||
UNS | W.Nr | |||||
N07750 | 2.4669 | |||||
Standard | ||||||
Bar | Forging | Sheet/Strip | Wire | |||
ASTM B637 | ASTM B637 | AMS 5542 AMS 5598 | AMS 5698 AMS 5699 |