Model | Epoxy resin A、Epoxy resin B |
viscosity(25℃) | 1000-1100mPa.s |
mixing ratio | By Bolume:1:1 or By Weight1:0.9 |
mixed viscosity(25℃) | 950-1000mPa.s |
initial curing time(25℃) | 4-6 hours |
fully cured time(25℃) | 10-24 hours |
Max pouring Thickness | 3-4 cm |
item | value |
CAS No. | 5888-33-5 7473-98-5 |
Other Names | Epoxy Crystal Glue |
MF | 227-561-6 231-272-0 |
EINECS No. | YLABJ-0002 |
Place of Origin | China |
Classification | Double Components Adhesives |
Main Raw Material | resin |
Usage | Construction, Fiber & Garment, Footwear & Leather, Packing, Transportation, Woodworking, Art |
Brand Name | oyowooa |
Model Number | YLABJ-0002 |
Type | epoxy resin art handmake |
color | crystal |
Packing | box |
Certificate | MSDS/TDS |
Curing condition | normal temperature |