Suitable material | Titanium or Cobalt-Chromium Alloy |
Application | crowns, copings and partial frames |
Usable construction volume | φ150 mm, H=80 mm |
Layer Thickness | 20-60μm |
Scan speed | Max 15m/s |
Produce speed | 12 brackets/3.5 hours |
Laser type | Yb-fiber laser; 300W*2 |
Laser point | 30-50μm |
Shielding Gas | Nirogen, Argon, <12L/min |
Working temperature | 18-30℃ |
Power | 3.5 KW |
Device dimension | 1070*670*1750mm |
Weight | 460kg |