Item
|
Testing Standards
|
Standard
|
Result
|
Finish
|
\
|
\
|
UV
|
Dimensional Stability after exposure to heat
|
EN 434 - 1994
|
<=0.25%
|
Longitudinal: 0.02%
Horizontal: 0.05%
|
Curling after exposure to heat
|
EN 434 - 1994
|
<=2.0mm
|
0mm
|
Residual indentation
|
EN ISO 24343 -1: 2012
|
\
|
Pass(0.01 mm)
|
Density
|
EN ISO 23996: 2012
|
\
|
1987.2 kg/m³
|
Flexibility
|
EN ISO 24344: 2012
|
\
|
10.8 mm
|
Water absorption
|
EN 15534 -1: 2014
|
\
|
0%
|
Impact resistance
|
EN 438 -2: 2016
|
\
|
Max. unbroken height: 1550 mm, no crack
|
Light ageing test Xenon-arc exposure
|
ISO 4892 -2: 2013
|
\
|
Pass
|
Staining and resistances to chemicals
|
EN ISO 26987: 2012
|
\
|
Pass
|
Formaldehyde emission
|
EN 717 -1: 2001
|
\
|
ND
|
VOC
|
EPA 5021A: 2014
|
\
|
ND
|