Name | Model | Application | Method of use | Characteristic | Process parameters | Specifications |
Titanium boron agent | Ti4OB4 | Adjust the composition of alloying elements to replace the aluminum intermediate alloy. | According to the production of alloy element content in the alloy and the results of the analysis before furnace, calculated at 95% of the recovery efficiency is good, need to add dose, after grilled slag, aluminum evenly dispersed bubble into the molten pool directly, after being small flame disappeared, should be appropriate to strengthen artificial stirring, make its spread evenly, and according to the actual situation, the spread of the guarantee time. | The elements are 75% and the silicon is 95%. The yield is greater than 95%. The solid yield of iron agent is over 90%. Shelf life is one year. |
Temperature: 740 ℃ to 760 ℃. Melt time: 15 to 30 minutes. |
1, 500 g/piece Density: 3.8-4.2 kg/cm after Si: 2.5 g/cm after |
Titanium agent | Ti75 | |||||
Manganese agent | Mn75 | |||||
Copper agent | Cu75 | |||||
Iron | Fe75 | |||||
Chromium agent | Cr75 | |||||
Nickel agent | Ni75 | |||||
Zinc | Zn75 | |||||
Fast solvent | Si95 |
Product List |
Aluminum Alloy Cu75 Copper Additive Tablets |
Aluminum Alloy Cr75 Chromium Additive Tablets |
Aluminum Alloy Fe75 Iron Additive Tablets |
Aluminum Alloy Ti75 Titanium Additive Tablets |
Aluminum Alloy Ti40B4 Titanium Boron Additive Tablets |
Aluminum Alloy Mn75 Manganese Additive Tablets |
Aluminum Alloy Ni75 Nickel Additive Tablets |
Aluminum Alloy Si95 Silicon Additive Tablets |
Aluminum Alloy Zn Zinc Additive Tablets |
Packing: | 50KGs Iron Drum or 1000KGs Jumb Bag or packing as per request. |
Storare: | Storing in sealed, dry and cool condition, not exposing to air for long time, avoiding moisture. |
Characteristics: | Pink powder, slightly soluble in inorganic acid, insoluble in water. |