At 1900°C sinter temperature and 70 Pa pressure, Jonye made BN block with density at 1.8-2.0g/cm³. With our own special grade HBN powder, Jonye hot-pressed BN has better physical property, good thermal conductivity. The block can hold 2000°C high temperature and it can resist big thermal vibration.