Concrete Floor Leveling cement
Introduction:
Self-leveling cement is a high technology content, technical aspects also more complex high-tech green products. It is a combination of active ingredients of the dry-blended powdery material, widely used, it can be used in industrial plants, workshops, warehousing, commercial stores, exhibition halls, gymnasiums, hospitals, all kinds of open spaces, offices, but also for home, Villa, cozy small space, can be used as decorative surface layer, may be used as wear-resistant substrate. It gives a strong, fast setting, free-flowing mix that can be applied from 1 – 6mm. Adding Flexmaster admixture will increase flexibility, durability and adhesion strength.
Features and Benefits:
A):Non shrink - Non cracking
B):High compressive and flexural strength
C): Good flow properties and quick to harden
D): Ready to use (Just add water)
Application:
Self-leveling cement widely used, can be used in industrial plants, workshops, warehousing, commercial stores, exhibition halls, gymnasiums, hospitals, all kinds of open space, office etc, but also for home, villa, cozy little space and so on. Can be used as decorative surface layer, may be used as wear-resistant substrate.
Thecnical Date:
(Temperature: 20-25, Relative Humidity: 48%-55%)
Mixing Ratio: power : water = 25kg:5.5L |
Compressive Resistance: About 15Mpa after 1 day; About 30Mpa after (EN196) 7 days; About 40Mpa after 28 days. |
Density of Dry Powder: about 1.3kg/L |
|
Density of freshly mixed glue: about 2.0kg/L |
Folding Strength: About 5Mpa after 1 day; About 8Mpa after (EN196) 7 days; About 12Mpa after 28 days. |
Working Time: (20) about 30 min |
Falling Ball Rigidity: About 50Mpa after 1 days; About 55Mpa after (Brine11) 7 days. About 80Mpa after 28 days. |
Time of Upper Finishing: about 24-48 hours |
|
Consumption: 1.6kg/m²/mm |
Rub fastness BS 8204:AR1 |
Construction method :
1.The substrate must be clean, dry firm and no any residue, then use Xindadi special interface agent to paint the base plane.
2. After about 2-6 hours, mixed with water before construction, be sure to strictly self-leveling cement: water25:6 ~ 6.5kg mixed. First 6 ~ 6.5kg of water into the bucket, then pour the product side down while stirring until a homogeneous mixture, lay up 1 minute, then stir once again briefly.
3. Pour the mixture into the construction area, a zigzag rake to move to a desired uniform thickness (thickness constructability 1-4mm).Before initial setting, use defoaming roller to exclude air which mixed in before.
Notice:
1. No excess water or it may decrease the compressive strength.
2. No strong wind and sun within 24 hours after construction.
Picture:
Shipping Picture:
Business Card: