Alloy | Chemical compositions% | ||||||||||||||
C | Cr | Mo | Nb | Al | Ti | B | Zr | ||||||||
In625/GH3625 | <0.1 | 20-23 | 8.0-10.0 | 3.15-4.15 | <0.4 | <0.4 | |||||||||
K418 | 0.08~0.16 | 11.5~ 13.5 | 3.8~4.8 | 1.8~2.5 | 5.5~6.4 | 0.5~1.0 | 0.008~0.020 | 0.06~0.15 | |||||||
In718/GH4169 | <0.08 | 17-21 | 2.8-3.3 | 4.75-5.5 | 0.2-0.8 | 0.65-1.15 | |||||||||
GH3536/HX | 0.05-0.15 | 20.5-23 | 8.0-10.0 | 0.2-1.0 | <0.5 | <0.15 | <0.01 | 0.05~0.15 | |||||||
In713C | 0.08~0.20 | 12.0~14.0 | 3.8~5.2 | 2.3~2.80 | 5.5~6.5 | 0.5~1.0 | 0.005~0.015 | 0.05~0.15 | |||||||
In713LC | 0.05~0.11 | 11.0~13.0 | 1.50~2.50 | 0.4~1.00 | |||||||||||
CoCrMo/F75 | <0.35 | 27-30 | 5.0-7.0 | / | / | / | / | / |
Alloy | Chemical compositions% | ||||||||||||||
Fe | Si | Mn | Cu | Co | S | P | Ni | ||||||||
In625/GH3625 | <5.0 | ≤0.5 | ≤0.5 | <0.07 | / | <0.015 | <0.015 | Bal. | |||||||
K418 | ≤1.0 | ≤0.5 | ≤0.5 | / | / | ≤0.01 | ≤0.015 | Bal. | |||||||
In718/GH4169 | Bal. | ≤0.35 | ≤0.35 | ≤0.3 | ≤1.0 | ≤0.015 | ≤0.015 | 50-55 | |||||||
GH3536/HX | 17-20 | ≤1.0 | ≤1.0 | ≤0.50 | 0.5-2.5 | ≤0.015 | ≤0.025 | Bal. | |||||||
In713C | ≤2.5 | ≤0.5 | <0.25 | ≤0.50 | ≤1.0 | ≤0.015 | ≤0.015 | ||||||||
In713LC | ≤0.50 | ≤0.20 | |||||||||||||
CoCrMo/F75 | <0.75 | <1.0 | <1.0 | / | Bal. | <0.01 | <0.01 | <1.0 |
Product Name | Nickel-based casting superalloy |
Application | Mainly used for high temperature castings of automobile turbines, blades, and engines |