0.5mm 1.0mm 1.5mm 2.0mm HDPE Geomembrane Pond Liner Dam Liner
Application :
1).0.5mm ,0.75mm,1.0mm thickness HDPE Geomembrane pond liner
dam liner,reservior pond liner,fish farming pond liner ,shrimp farm pond liner,artificial lake liner
2).1.0mm,1.5mm,2.0mm thickness HDPE Geomembrane pond liner
Landfill,waste water treatment and mining
Features :
1.lowest permeability
2.high tensile strength
3.excellent chemical resistance
4.easy to install and shippment
5.longer service lifetime
6.save cost
Details :
1) Thickness : 0.2mm - 2.5mm.
2) Width : Within 8 m (1m-8m).
3) Length : 50m-200m/roll (as request).
4) Material : HDPE,( LDPE ).
5) Color : Black , white , red , blue , or as required.
6) Optional surface : smooth surface or Textued surface
Spec Properties |
GM0.5 |
GM0.75 |
GM1.0 |
GM1.5 |
GM2.0 |
Thickness |
0.50 mm |
0.75 mm |
1.00 mm |
1.50 mm |
2.00 mm |
Density ( ≥)
|
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
0.940 g/cc |
Tensile Properties ( ≥) • yield strength • break strength • yield elongation • break elongation |
7 kN/m 10kN/m — 600% |
10 kN/m 15kN/m — 600% |
13 kN/m 20 kN/m 11% 600% |
20 kN/m 30 kN/m 11% 600% |
26 kN/m 40 kN/m 11% 600% |
Tear Resistance ( ≥) |
56 N |
84 N |
115 N |
170 N |
225 N |
Puncture Resistance ( ≥) |
120 N |
180 N |
240 N |
360 N |
480 N |
Carbon Black Content ( ≥) |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
2.0-3.0% |
Oxidative Induction Time(OIT) Standard OIT ( ≥) |
60 min. |
60 min. |
60 min. |
60 min. |
60 min. |